Research on Corrosion Life Evaluation Method of Trackside Equipment in High Salt and High Humidity Environment
Bai Zhiwei1, Yang Shenlin1, Zhang Wei2, 3, Li Lanxin2, 3
1. Signal & Telecom Division, China Railway Guangzhou Group Co., Ltd., Guangzhou 510088, China,;
2. CRSC Research & Design Institute Group Co., Ltd., Beijing 100070, China;
3. Beijing Engineering Technology Research Center of Operation Control Systems for High Speed Railways, Beijing 100070, China
Bai Zhiwei, Yang Shenlin, Zhang Wei, Li Lanxin. Research on Corrosion Life Evaluation Method of Trackside Equipment in High Salt and High Humidity Environment[J]. Railway Signalling & Communication Engineering, 2021, 18(3): 12-17.
[1]赵自信.ZPW-2000A无绝缘移频自动闭塞系统的技术综述[J].铁路通信信号设计,2003(z1):12-19.
[2]徐宗奇,阳晋.我国轨道电路发展历程及现状[J].铁道通信信号,2019,55(z1):55.
[3] Kong Decheng, Dong Chaofang, Xiao Kui, et al. Effect of Temperature on Copper Corrosion in High-Level Nuclear Waste Environment[J].Transactions of Nonferrous Metals Society of China, 2017, 27(6): 1431-1438.
[4] Oh K, Ahn S, Eom K, et al. A Study on the Localized Corrosion and Repassivation Kinetics of Fe-20Cr-xNi (x=0–20 Wt%) Stainless Steels via Electrochemical Analysis[J].Corrosion Science, 2015(7): 158-168.
[5] Yange Y, Cui Z, Chen J, et al. Influence of Hydrostatic Pressure on the Pitting Behavior of Fe-20Cr Alloy[J]. Journal of Chinese Society for Corrosion and Protection, 2009, 29(6): 415-420.
[6]国家铁路局.TB10621—2014 高速铁路设计规范[S].北京:中国铁道出版社,2014.
[7]中国钢铁工业协会.GB19292.1-2018 金属和合金的腐蚀大气腐蚀性分类[S].北京:中国标准出版社, 2018.
[8]中国钢铁工业协会.GB/T20854-2007 金属和合金的腐蚀循环暴露在盐雾、“干”和“湿”条件下的加速试验[S].北京:中国标准出版社, 2007.